Pyrolytic Boron Nitride (PBN)

Pyrolytic Boron Nitride Products

Property Unit Value
Lattice constant micro; m a:2.504×10-10 c:6.692×10-10
Apparent density g/cm3 2.0 -2.21(board) 2.0 -2.17(crucible)
Helium transmissivity cm3/S 1×10-12
Solidity by microscope N/mm2 691.88
Volume resistivity Ω·cm 3.11×1011
Tensile strength (Strength “C”)N/mm2 153.86
Bending strength (Strength “C”)N/mm2 , a: 243.63
(Strength⊥“C”)N/mm2 , c: 197.76
Elasticity modulus N/mm2 235690
Pyroconductivity W/m·k “a” direction “c“ direction
W/m·k (200°) 60 2.60
W/m·k (900°) 43.70 2.80
Dielectric strength (room temperature) KV/mm 56
Purity 99.99-99.999/td>


Features & Advantages:

  1. Non-toxic.
  2. Non-wetting
  3. High purity(>99.99%) compared with hot pressing BN
  4. High thermal conductivity.
  5. High electrical resistance.
  6. Excellent thermal shock resistance.
  7. High working temperature (>2000℃).
  8. Non-reactive to most other compounds

Typical Applications

  1. OLED Production
  2. MOCVD Heater
  3. Polycrystalline Synthesis
  4. Molecular Beam Epitaxy (MBE)
  5. Compound Semiconductor Crystal Growth
  6. Satellite Communication TWT